MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Rogers Arlon MT920-10#3.3-P1 0.020" (0.508 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave  (discontinued **)
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description:
0.020” thick x 1.0” wide x 3.33 yards long, Rectangular cross-section, Silicone, Self-Fusing Tape.

Design/Construction:
Interleave: Polyethylene
Rubber: Cured Self-Fusing Silicone Rubber
Cross-Section: 1.0” Wide Triangular

Meets US Military Specification A-A59163 (supersedes Mil-I-46852C) except for sampling level and packaging. The following tests are conducted on one roll from each lot of tape per A-A-59163: Thickness, Width, Bond Strength, Tensile Strength, Elongation, Dielectric Strength, and Water Absorption.

Product Use: Multi-use tape

Appearance: Various colored silicone rubber tape on polymer liner.

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccSilicone Property; Arlon SQA-TMS-024
Water Absorption 1.7 %Arlon SQA-TMS-016
Thickness 2.50 milPolyethylene, Interleave
 20.0 milRubber; Arlon SQA-TMS-003
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55Silicone Property; ASTM D2240
Tensile Strength 1130 psiSilicone Property; ASTM D412
Elongation at Break 560 %Silicone Property; ASTM D412
Peel Strength 3.10 pliBond Strength; Arlon SQA-TMS-015
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 870 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -60.0 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 21.1 °C
From date of manufacture
 
Descriptive Properties
ColorBlack
 Blue
 Green
 Natural
 Vibrant Red
 Yellow

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARL563 / 125749

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.