MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Brueggemann Chemical Nyrim® 1000 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Conditioned at 23°C and 50% Relative Humidity.

Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) technology. Nyrim® is a registered trademark.

Information provided by the manufacturer, Brueggemann Chemical.

Key Words: RIM materials
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Moisture Absorption at Equilibrium 3.1 %3.1 %DIN 53714: 23°C, 50% Relative Humidity
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7474ISO 868
Tensile Strength, Ultimate 49.0 MPa7110 psiISO 527
Elongation at Break 250 %250 %ISO 527
Modulus of Elasticity 1.197 GPa173.6 ksiISO 527
Flexural Modulus 1.163 GPa168.7 ksiISO 178
Shear Modulus 0.520 GPa75.4 ksitorsional
Izod Impact, Notched (ISO) 35.0 kJ/m²16.7 ft-lb/in²ISO 180, Ductile break
 4.00 kJ/m²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
Brittle break; ISO 180
Charpy Impact, Notched 3.10 J/cm²14.8 ft-lb/in²DIN 53453, Ductile break
 0.800 J/cm²
@Temperature -40.0 °C
3.81 ft-lb/in²
@Temperature -40.0 °F
Brittle break; DIN 53453
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+9 ohm-cm5.00e+9 ohm-cmDIN 53482
Surface Resistance 4.00e+8 ohm4.00e+8 ohmDIN 53482
Dielectric Constant  4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
DIN 53483
 15.3
@Frequency 50 Hz
15.3
@Frequency 50 Hz
DIN 53483
Dielectric Strength 13.0 kV/mm330 kV/inDIN 53481
Dissipation Factor 0.10
@Frequency 1e+6 Hz
0.10
@Frequency 1e+6 Hz
DIN 53483
Comparative Tracking Index 400 V400 VDIN IEC 112 / VDE 030 t1
 
Thermal PropertiesMetricEnglishComments
Melting Point 214 °C417 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DSM Fibre Intermediates Nyrim® 3000 (Dry)
Brueggemann Chemical Nyrim® 1000 (Dry)
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 20 pcf, MDI-based 2-Component Liquid System
Covestro Baydur® 646 Polyurethane Structural Foam RIM, Density 25 pcf, MDI-based 2-Component Liquid System
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 30 pcf, MDI-based 2-Component Liquid System

PDSMN006 / 31478

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.