MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
1,2,3-Trichloropropane, C3H5Cl3
Categories: Fluid; Solvent

Key Words: C3H5Cl3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.389 g/cc
@Temperature 20.0 °C
Viscosity 2.541 cP
@Temperature 20.0 °C
Dynamic Viscosity
Molecular Weight 147.432 g/mol
Vapor Pressure 2.384 torr
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 39.0 atm
Critical Temperature 378 °C
Critical Density 0.424 g/cc
Critical Molar Volume 348 cm³/mol
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 260.5 J/g
Specific Heat Capacity 0.762 J/g-°C
@Temperature 25.0 °C
Vapor
Thermal Conductivity 0.1092 W/m-K
@Temperature 20.0 °C
Melting Point -14.7 °C
Boiling Point 155.9 °C
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.1246
Antoine's Vapor Pressure B Parameter3417.27
Antoine's Vapor Pressure C Parameter-69.15
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)598-77-6
Chemical FormulaC3H5Cl3
Critical Compressibility (Zc)0.25
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A818.63
Dynamic Viscosity Parameter B342.88
Henry's Law Constant (atm m3/mol)0.526
Molar Heat Capacity (298K)112.355 J/mol-K
Molar Heat Capacity of Vapor a Parameter26.8655
Molar Heat Capacity of Vapor b Parameter0.362
Molar Heat Capacity of Vapor c Parameter-0.0002785
Molar Heat Capacity of Vapor d Parameter8.782E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

VORGS353 / 99700

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.