MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Celanex® 3210 Polyester (PBT), 20% Glass-Fiber
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant

Material Notes: Flame retardant

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.62 g/ccASTM D792
Water Absorption 0.070 %ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90ISO 2039-2
Tensile Strength, Ultimate 115 MPaISO 527
Elongation at Break 3.0 %ASTM D638
Flexural Strength 170 MPaISO 178
Flexural Modulus 8.00 GPaISO 178
Izod Impact, Notched (ISO) 0.500 J/cm²ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.8
@Frequency 100 Hz
Dielectric Strength 19.0 kV/mm
@Thickness 3.17 mm
50% RH; ASTM D149
Dissipation Factor 0.0020
@Frequency 100 Hz
Comparative Tracking Index 330 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 223 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 203 °CISO 75
Flammability, UL94 V-0
@Thickness 0.800 mm
UL94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celanex® 5201 15% Fiberglass Reinforced Polyester
Celanese Celanex® 3225HRT PBT, 15% Fiberglass Reinforced
Celanese 1503 FDA Nylon 6/6, 33% Glass-Fiber Reinforced, Dry As Molded
Celanese 1503 FDA Nylon 6/6, 33% Glass-Fiber Reinforced, at 50% RH
Celanese Celanex® 3318 PBT, 30% Glass Reinforced

PHCT22 / 45662

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.