HD 9856BA is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856BA exhibit a unique combination of stiffness and environmental stress cracking resistance. These properties, coupled with excellent processability on both continuous and intermittent equipment, afford significant lightweighting and/or fast cycling potential in many applications. HD 9865BA contains an antistat which may be used in contact with limited types of food. Information provided by ExxonMobil Chemical |