MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gromax CCP PBT 1100-600S
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Product Description: PBT unreinforced high viscosity injection molding grade.

Characteristics:

  • Excellent electrical property
  • Excellent temperature resistance, high heat distortion temperature.
  • Excellent mechanic and chemical property
  • Excellent weatherability
  • Excellent wear property
  • Excellent moldability
  • High resistance to fuels, oil, fats and many solvents

    Information provided by Gromax Enterprises Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Moisture Absorption 0.0600 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.012 - 0.018 cm/cm
@Thickness 1.60 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 117ASTM D785
Tensile Strength 540 kg(f)/cm²ASTM D638
Elongation at Break 200 %ASTM D638
Flexural Strength 84.0 MPaASTM D790
Flexural Modulus 24000 kg(f)/cm²ASTM D790
Izod Impact, Notched >= 3.00 kg-cm/cm
@Thickness 6.35 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+13 ohmASTM D257
Dielectric Constant 3.3
@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
@Thickness 2.00 mm
ASTM D149
Dissipation Factor 0.0010
@Frequency 60 Hz
ASTM D150
Arc Resistance 120 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°CASTM D696
Melting Point 225 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 155 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 230 - 260 °C
Nozzle Temperature 245 - 250 °C
Mold Temperature 30.0 - 100 °Csuitable temperature 40-60°C
Injection Pressure 50.0 - 100 MPa
Hold Pressure 30.0 - 70.0 MPa
Back Pressure 0.000 - 0.300 MPa
Screw Speed 60 - 120 rpmto be chosen in such a way that plasticizing time is just within cooling time
 
Descriptive Properties
Injection Ratemiddle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gromax CCP PBT 1100-104S
Gromax CCP PBT 1100-220S
Gromax CCP PBT 1100-211X
Gromax CCP PBT 1100-630S
Gromax CCP PBT 1200-211E

PGROM018 / 147831

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.