MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Materion Brush 1915™ Hard Temper Rod, 0.050" - 0.375"
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Information supplied by Brush Wellman Engineered Materials.

Treatment required for max strength: as supplied

Brush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered specifically for automatic screw machine applications, Brush 1915 provides high strength and good machinability. Brush Wellman's quality system provides an excellent surface finish, close diameter control, and tight compositional control in Brush 1915. The properties of brush 1915 make it an ideal material for machined electrical contacts.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: UNS C19150
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.88 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 380 - 510 MPa
Tensile Strength, Yield 310 - 480 MPa
Elongation at Break 5.0 - 20 %
Modulus of Elasticity 124 GPa
Machinability 75 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000310 ohm-cm(55% IACS Conductivity)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.7 µm/m-°C
@Temperature 20.0 - 200 °C
Thermal Conductivity 210 W/m-K
Melting Point 1038 - 1082 °C
Solidus 1038 °C
Liquidus 1082 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 98 %as balance
Lead, Pb 0.50 - 1.0 %
Nickel, Ni 0.80 - 1.2 %
Phosphorus, P 0.15 - 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Uninhibited Naval brass, UNS C46400, O61 Temper tubing
Phosphorized Naval brass, UNS C46700, H01 (8%) Temper 25 mm rod/bar
Materion Brush® 1916 Machinable Copper Nickel Alloy Rod, Temper A (UNS C19160)
Materion Brush 1915™ AT Temper Rod
Materion Brush 1915™ Annealed Temper Rod

NBB272 / 15121

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.