MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Eastman Piccotac™ 1100 Hydrocarbon Resin
Categories: Polymer

Material Notes: Product Description: Piccotac™ 1100 hydrocarbon resin is a 100°C softening point, thermoplastic, low molecular weight, aliphatic C5 resin. Derived largely from mixed monomers of petroleum origin, it is characterized by its light color, excellent balance of tack and of adhesive and cohesive properties, heat resistance, and wide compatibility and solubility. Piccotac™ 1100 hydrocarbon resin is stabilized by addition of 0.10% antioxidant. It is designed primarily for use in pressure sensitive adhesives and hot melt adhesives and coatings.

Application/Uses:

  • Automotive refinish
  • Building and Construction
  • Hot Melt Adhesives
  • Nonwovens
  • Packaging
  • Pressure sensitive adhesives
  • Solventborne Adhesives
  • Tapes and Labels
  • Wax Modification
Key Attributes:
  • Aliphatic C5 resin
  • Excellent adhesion to natural rubber based adhesives
  • Excellent color and color stability
  • Excellent peel and tack properties
  • Limited compatibility with styrene-isoprenestyrene (SIS) block copolymersInformation provided by Eastman
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity  1000 cP
@Temperature 170 °C
1000 cP
@Temperature 338 °F
Melt
 10000 cP
@Temperature 135 °C
10000 cP
@Temperature 275 °F
Melt
 100000 cP
@Temperature 120 °C
100000 cP
@Temperature 248 °F
Melt
Molecular Weight 950 g/mol950 g/molMn
 2900 g/mol2900 g/molMw. Mw/Mn ratio = 3
 8250 g/mol8250 g/molMz
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 46.0 °C115 °F
Ring & Ball Softening Point 100 °C212 °FASTM E28
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 3.03.0
 
Descriptive Properties
Cloud Point62°CDACP
 96°CMMAP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5512 / 222706

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.