MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Scotch-Weld™ 4475 Industrial Adhesive
Categories: Polymer; Adhesive

Material Notes:

Features:

  • Dries quickly to a firm bond
  • Excellent resistance to water, plasticizer migration, many detergent and soap solutions, oils and greases
  • A general purpose adhesive for bonding most vinyls, ceramics, glass, leather and cloth to a variety of substrates.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 41 - 45 %41 - 45 %
Brookfield Viscosity 6500 - 10500 cP6500 - 10500 cPRVF #5 sp @ 20 rpm @ 80°F
 
Mechanical PropertiesMetricEnglishComments
Peel Strength  1.23 kN/m
@Temperature 82.0 °C,
Time 1.81e+6 sec
7.00 pli
@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
 2.28 kN/m
@Temperature 24.0 °C,
Time 86400 sec
13.0 pli
@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
 2.98 kN/m
@Temperature 66.0 °C,
Time 1.81e+6 sec
17.0 pli
@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
 3.86 kN/m
@Temperature -34.0 °C,
Time 1.81e+6 sec
22.0 pli
@Temperature -29.2 °F,
Time 504 hour
180°, Canvas/Steel
 4.21 kN/m
@Temperature 24.0 °C,
Time 259000 sec
24.0 pli
@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
 4.82 kN/m
@Temperature 24.0 °C,
Time 432000 sec
27.5 pli
@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
 5.70 kN/m
@Temperature 24.0 °C,
Time 605000 sec
32.5 pli
@Temperature 75.2 °F,
Time 168 hour
180°, Canvas/Steel
 6.14 kN/m
@Temperature 24.0 °C,
Time 1.21e+6 sec
35.0 pli
@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
 7.71 kN/m
@Temperature 24.0 °C,
Time 1.81e+6 sec
44.0 pli
@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
 
Thermal PropertiesMetricEnglishComments
Flash Point -6.60 °C20.1 °FCC
 
Processing PropertiesMetricEnglishComments
Shelf Life 15.0 Month15.0 Month
 
Descriptive Properties
AppearanceClear
BaseSynthetic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34109 / 168856

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.