MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
INEOS Styrolution Novodur® M210TF Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Novodur® M210TF is medium impact, high gloss injection molding grade designed for toy application. M210TF is in compliance with food contact regulations. Medium impact, High gloss, Meets food contact requirements. Applications: Toys, Application with food contact requirements

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmISO 294-4
Melt Flow 30 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 90.0 MPaISO 2039-1
Tensile Strength, Yield 42.0 MPaISO 527
Elongation at Break >= 15 %ISO 527
Elongation at Yield 2.4 %ISO 527
Tensile Modulus 2050 MPaISO 527
Flexural Strength 60.0 MPaISO 178
Flexural Modulus 2050 MPaISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 17.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 17.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.9
@Frequency 100 Hz
IEC 60250
 2.9
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0060
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°CISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °Cannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 95.0 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 260 °CISO 294
Mold Temperature 60.0 - 80.0 °CISO 294
Injection Velocity 240 mm/secISO 294
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos ABS Lustran® M205FC ABS Pellets, Injection Molding Grade
Denka CL-430 Transparent Resin Polymer (MABS) ABS
INEOS Styrolution Terluran® HH-112 Q109 ABS
INEOS Styrolution Novodur® Ultra 4000PG Acrylonitrile Butadiene Styrene / Polycarbonate (ABS/PC)
INEOS Styrolution Novodur® P2HE ABS, Extrusion Grade

PSTYR9820 / 216047

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.