MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aclo Accutech Polyethylene HD0232G20CV High Density Glass Reinforced Chemically Coupled
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Glass fiber Filled

Material Notes: Approved to GMP.PE.018 Black A12438

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D792
Linear Mold Shrinkage 0.0040 cm/cmASTM D955
Melt Flow 0.20 g/10 minASTM D1238
Ash 18 - 22 %ASTM D2584
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 75ASTM D785
Tensile Strength, Yield 5510 psiASTM D638
Elongation at Break 5.0 %ASTM D638
Tensile Modulus 362500 psiASTM D638
Flexural Strength 4930 psiASTM D790
Flexural Modulus 362500 psiASTM D790
Izod Impact, Notched 2.00 ft-lb/inASTM D256
Izod Impact, Unnotched 8.00 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 257 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 203 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accutech Polyethylene HD0234G10UVL High Density Glass Reinforced UV Stabilized
Aclo Accutech Polyethylene HD0234G40UVL High Density Glass Reinforced UV Stabilized
Bamberger Polymers Bapolene® 0760 High Density Polyethylene, Blow Molding Grade
A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable

PACLO089 / 22344

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.