MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cronifer 1925 hMO High-Nitrogen Austenitic Stainless Steel, Annealed Bar, Wire, UNS N08925
Categories: Metal; Ferrous Metal; Stainless Steel

Key Words: ASTM B649
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 600 MPa
Tensile Strength, Yield 300 MPa
Elongation at Break 40 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Chromium, Cr 24 - 26 %
Copper, Cu 0.80 - 1.5 %
Iron, Fe 42.705 - 50.1 %As Balance
Manganese, Mn <= 1.0 %
Molybdenum, Mo 6.0 - 7.0 %
Nickel, Ni 19 - 21 %
Nitrogen, N 0.10 - 0.20 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel 309 Austenitic Stainless steel
AK Steel 304 Austenitic Stainless steel
AISI Type S24100 Stainless Steel 25 mm mill-annealed bar
AISI Type S24000 Stainless Steel, annealed bar up to 200 mm diameter
AISI Type S21904 (Alloy 21-6-9) Stainless Steel, 25 mm annealed round, tested in longitudinal direction

MQZ9920 / 172155

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.