MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

TOSAF Compounds Tosaf ME80000I Polyolefin, Masterbatch
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: ME80000I White MB is suitable for coloring films and injection parts made of Various Types of polyolefins. Design especially for indoor items.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

RoSH Compliance: RoSH Compliant

Additives Category: Masterbatch – Pigment – White

Carrier Resin: Polyethylene or ethylene-olefin copolymer (PE)

Recommended for Use In: Polyethylene or ethylene-olefin copolymer (PE); Polypropylene or propylene-olefin copolymer (PP)

Form: Pellets/Granules

White Pigment Composition (60%): Titanium dioxide (TiO2)

Chemical Description: Titanium dioxide

State at Room Temperature: Solid

Information provided by TOSAF Compounds Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.21 g/cc0.0798 lb/in³
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 110 °C>= 230 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 300 °C<= 572 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTOSAF1503 / 312196

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.