MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SCG Chemicals EL-Lene™ L2009F Linear Low Density Polyethylene Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Key Characteristics:
  • High productivity
  • Good optical properties
  • Can be blended with HDPE and LDPE to improve tear resistance and seal strength
  • Contains 1000 ppm slip agent and 700 ppm antiblocking agent

Recommended Applications:

  • Film for heavy duty bag, industrial bag, rice bag, sugar bag, frozen bag
  • Agricultural film
  • Construction film

Information provided by SCG Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.919 g/cc0.919 g/ccASTM D1505
Environmental Stress Crack Resistance >= 1000 hour
@Temperature 50.0 °C
>= 1000 hour
@Temperature 122 °F
F50, 25% Igepal; ASTM D1639
Thickness 38.0 microns1.50 mil
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 12.0 MPa1740 psiASTM D882
Film Tensile Strength at Yield, TD 14.0 MPa2030 psiASTM D882
Film Elongation at Break, MD 1000 %1000 %ASTM D882
Film Elongation at Break, TD 1200 %1200 %ASTM D882
Secant Modulus, MD 0.260 GPa37.7 ksiASTM D882
Secant Modulus, TD 0.270 GPa39.2 ksiASTM D882
Elmendorf Tear Strength, MD 5.71 g/micron145 g/milASTM D1922
Elmendorf Tear Strength, TD 14.6 g/micron370 g/milASTM D1922
Dart Drop 3.40 g/micron86.4 g/milASTM D1709
Dart Drop Test 130 g0.287 lbASTM D1709
Film Tensile Strength at Break, MD 37.0 MPa5370 psiASTM D882
Film Tensile Strength at Break, TD 34.0 MPa4930 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 122 °C252 °FASTM D2117
Vicat Softening Point 102 °C216 °FASTM D1525
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Haze 16 %16 %ASTM D1003
Gloss 52 %52 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Extruded

PSCGC939 / 120693

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.