MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lotte Chemical Titan TITANPRO® PM202 Polypropylene homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvant meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use.

Applications:

  • High speed fine denier fiber production.
  • Spun-bond fibers.
  • Multifilament fibers.

Advantages:

  • High melt flow.
  • Good draw-ability.
  • High gloss.
  • Narrow molecular weight distribution.
  • Excellent spinning performance.

Fabrication:

  • Equipment - general extrusion machines.
  • Techniques - standard processing.

Information provided by Titan Chemicals

CAS# 9003-07-0

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Base Resin Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Water Absorption 0.020 %0.020 %after 24 hrs; ASTM D570
Base Resin Melt Index 25 g/10 min
@Temperature 230 °C
25 g/10 min
@Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100100ASTM D785A
Tensile Strength, Yield 32.4 MPa4700 psiASTM D638
Elongation at Yield 12 %12 %ASTM D638
Flexural Modulus 1.27 GPa184 ksiASTM D790B
Izod Impact, Notched 0.294 J/cm0.551 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C203 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Chemical Titan TITANPRO® PM655 Polypropylene homopolymer
Lotte Chemical Titan TITANPRO® PX617 Polypropylene homopolymer
Lotte Chemical Titan TITANPRO® PD943 Polypropylene homopolymer
Lotte Chemical Titan TITANPRO® PD855 Polypropylene homopolymer
Lotte Chemical Titan TITANPRO® PD701 Polypropylene homopolymer

PTITAN10 / 70376

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.