MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Tefzel® 207 Resin Modified ETFE
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: DuPont™ Tefzel ® 207 fluoropolymer is a special-purpose resin available in translucent, 2.5 mm (0.1 in) pellets. Compared with other grades of Tefzel ®, it has a higher flow rate but still maintains a service temperature of 150°C (302°F).

Tefzel ® 207 and the other Tefzel ® fluoropolymers are melt processible, modified copolymers of ethylene and tetrafluoroethylene. They are high-performance resins that can be processed at relatively high rates compared with fluorocarbon resins. They are mechanically tough and offer an excellent balance of properties. The relatively high flow rate (see Table 1) of Tefzel ® 207 makes it uniquely suitable for high-speed processing, especially for extruded coatings and injection molding of slender, thin-walled or intricate shapes. Properly processed products made from neat Tefzel ® 207 are inert to most solvents and chemicals, hydrolytically stable, and weather resistant. Recommended upper service temperature is 150°C (302°F); useful properties are retained at cryogenic ranges. The level and stability of dielectric properties are excellent and the flame rating is V-0 by the UL94 method. Mechanical properties include outstanding impact strength, cut-through, and abrasion resistance.

Statements, or data, regarding behavior in a flame situation are not intended to reflect hazards presented by this or any other material when under actual fire conditions.

Applications

Tefzel ® 207 is ideal for many end products, including electrical components such as sleeving, coil forms, sockets, connectors, and switches; lab ware such as tubing, valves, containers, and fasteners; battery or instrument components that require chemical inertness; and mechanical parts. The high melt flow rate of this product makes it ideal for injection molding and thin wall extrusion.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015.

Key Words: Ethylene Tetrafluoroethylene Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 g/ccASTM D792
Water Absorption 0.0070 %24 hours; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 72ASTM D2240
Tensile Strength, Ultimate 40.0 MPaASTM D3159
Elongation at Break 300 %ASTM D3159
Flexural Modulus 1.00 GPaASTM D790
Izod Impact, Notched NBASTM D256
Coefficient of Friction 0.30 - 0.40ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+17 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+15 ohmASTM D257
Dielectric Constant 2.6 - 2.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 66.92 kV/mm
@Thickness 0.250 mm
ASTM D149
Dissipation Factor 0.0090
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 122 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Melting Point 267 °CASTM D3418
Maximum Service Temperature, Air 150 °C
Flammability, UL94 V-0
Oxygen Index 30 - 32 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 302 - 323 °CCure Temperature
 
Descriptive Properties
20% Hydrochloric Acid Transmission, g/100sq in.<0.02
50% Sodium Hydroxide Transmission, g/100sq in.<.02
Acetic Acid Transmission, g/100sq in.0.41
Acetone Transmission, g/100sq in.0.95
Acetophenone Transmission, g/100sq in.0.5
Benzene Transmission, g/100sq in.0.64
Carbon Tetrachloride Transmission, g/100sq in.0.31
Chemical/Solvent ResistanceExcellent
Ethyl Acetate Transmission, g/100sq in.0.76
Folding Endurance, # cycles, .18-.20 mm10-27 E3
Heat of Combustion J/g13700ASTM D240
Hexane Transmission, g/100sq in.0.56
Piperidine Transmission, g/100sq in.0.04
Red Fuming Nitric Acid Transmission, g/100sq in.7.5-1.4
Salt Spray Resistance on aluminum, Hours1000
Sulfuric Acid Transmission, g/100sq in.0.00001
Water Transmission, g/100sq in.0.4
Weather Resistance15Years unaffected in Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Tefzel® 750 Fluoropolymer Resin
Chemours Tefzel® 200 Resin Modified ETFE
Chemours Tefzel® 280 Resin Modified ETFE
Chemours Tefzel® 210 Resin Modified ETFE
Chemours Tefzel® 2195 Fluoropolymer Resin

PDU928A / 33356

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.