System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
DuPont Mobility and Materials BETASEAL™ 16080N Adhesive
Categories:
Polymer
;
Adhesive
;
Thermoset
Material Notes:
Primerless to paint, one-component, fast curing, high viscosity adhesive.
Information provided by DuPont Performance Polymers.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.26
g/cc
0.0455
lb/in³
ISO 1183
Solids Content
>= 99 %
>= 99 %
Viscosity Measurement
25 - 50
25 - 50
sec.; Cup Viscosity; 20 g sample
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
65
65
ASTM D 2240
Elongation at Break
500 %
500 %
ASTM D 412
Tensile Modulus
0.00300
GPa
0.435
ksi
ISO 527-1/-2
Stiffness Modulus
>=
0.00100
GPa
>=
0.145
ksi
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
100
°C
212
°F
Temperature stability
Minimum Service Temperature, Air
-40.0
°C
-40.0
°F
Temperature stability
Processing Properties
Metric
English
Comments
Processing Temperature
18.0
-
35.0
°C
64.4
-
95.0
°F
Shelf Life
6.00
Month
@Temperature 0.000 - 40.0 °C
6.00
Month
@Temperature 32.0 - 104 °F
From date of manufacture in unopened containers
Descriptive Properties
Basis
Polyurethane
Color
Black
Polymer
Adhesive
Sagging
0°
Skinning time
10 to 45
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PDTF9151c / 295956
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.