MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

TPC Group TPC 545 Highly Reactive Grade Polyisobutylene
Categories: Polymer

Material Notes: Characteristics: TPC 545 is colorless (water white), has very low moisture transition rates, is non-corrosive, can be used for emulsions and is hydrophobic with a molecular weight range of 300 - 500. TPC 545 is a highly reactive polyisobutylene (HRPIB) grade, which means that greater than 80% of its double bonds are in the terminal position of the molecule (alpha).

Applications: TPC 545 can be used for a variety of applications such as: fuel additives, lubricant oil additives, emulsifiers, 2 stroke engine oils, viscosity modifiers, pour point depressants, corrosion inhibitors, tackifiers, asphalt/bitumen, sealants, polypropylene films, personal care products, drilling fluids, metal working fluids, cables and compressor oils and PIBSA reactions.

General: HR-PIB is especially valued in the fuel and lubricant market as it delivers improved end product performance to the consumer and better manufacturing economics for the additive supplier. Processing with HR-PIB also produces less char during manufacture and the derivative products are used to improve funal lubricant and fuel performance. TPC Group offers the broadest portfolio of PIB products to the market and is a major supplier to many different markets, including fuels and lubricants, caulks, sealants, adhesives, packaging, greases and emulifiers.

Packaging: TPC 545 is typically sold in railcar quantities, but trucks and isocontainers are also available.

Information provided by TPC Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.800 - 0.900 g/cc
@Temperature 15.6 °C
0.800 - 0.900 g/cc
@Temperature 60.1 °F
ASTM D4052
Viscosity Measurement 100100Index; ASTM D2270
Kinematic Viscosity 10 - 25 cSt10 - 25 cStASTM D445
 15 cSt
@Temperature 100 °C
15 cSt
@Temperature 212 °F
ASTM D445
 31 cSt
@Temperature 70.0 °C
31 cSt
@Temperature 158 °F
ASTM D445
 105 cSt
@Temperature 40.0 °C
105 cSt
@Temperature 104 °F
ASTM D445
 500 cSt
@Temperature 20.0 °C
500 cSt
@Temperature 68.0 °F
ASTM D445
Molecular Weight 350 - 550 g/mol350 - 550 g/mol
Evaporation Loss 6.6 %
@Temperature 99.0 °C,
Time 36000 sec
6.6 %
@Temperature 210 °F,
Time 10.0 hour
ASTM D972
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.10<= 0.10[mg KOH/g]; ASTM D974
 
Electrical PropertiesMetricEnglishComments
Dielectric Breakdown 50000 V50000 VASTM D877
Dissipation Factor 0.000080
@Temperature 100 °C
0.000080
@Temperature 212 °F
ASTM BS5737
 
Thermal PropertiesMetricEnglishComments
Pour Point -39.0 °C-38.2 °FASTM D97
Flash Point >= 130 °C>= 266 °FCOC; ASTM D92
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.47851.4785ASTM D1218
Haze <= 4.0 %<= 4.0 %Photometric; ASTM D6181
 
Descriptive Properties
AppearanceClear and Bright
Bromine Number33.6 g Br2/100gASTM 1159
Color<70APHA, ASTM D1209
Content<1 ppmChlorine, ASTM D4327
 <1 ppmSulfur, ASTM D2622
 <1 ppmAromatics
 >75%Alpha Vinylidene Content
 25 ppmWater, ASTM D1533
Power Factor8E-05100°C, ASTM D924
Saponification Number<1 mg KOH/gASTM D94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTPCG009 / 320511

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.