MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik Kanthal Super NC Molybdenum disilicide
Categories: Metal; Ferrous Metal

Material Notes: Kanthal Super NC is a heating element with special features, designed to meet the demand for clean process heating in the research and electronics industries. Scaling of the element surface, which occurs in all heating elements, is reduced to a minimum. The metal content is also reduced which means less diffusion into the furnace atmosphere from the element. The content of Fe, Ni and Cu (and other elements on request) can be verified and confirmed in a certificate of analysis. The electrical properties are the same as for Kanthal Super 1800.

Special features:

  • Extra clean and adherent surface glaze
  • Lower metal content
  • Certificate of analysis
  • Can be used in air/oxidizing atmospheres up to 1800°C (3270°F)
  • 25% higher bending strength at room temperature compared to Kanthal Super 1800
  • Standard and specially designed elements
Typical area of application includes all type of clean process in the research and electronics industries.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.60 g/cc0.202 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 75.0 - 125 MPa
@Temperature 1500 °C
10900 - 18100 psi
@Temperature 2730 °F
Elongation at Break 9.0 %9.0 %
Flexural Strength 405 - 495 MPa58700 - 71800 psi
Compressive Strength 1400 - 1500 MPa203000 - 218000 psi
Fracture Toughness 3.00 - 4.00 MPa-m½2.73 - 3.64 ksi-in½
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.00 - 8.00 µm/m-°C3.89 - 4.44 µin/in-°F
Specific Heat Capacity 0.420 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity  15.0 W/m-K
@Temperature 600 - 1200 °C
104 BTU-in/hr-ft²-°F
@Temperature 1110 - 2190 °F
 30.0 W/m-K
@Temperature 20.0 - 600 °C
208 BTU-in/hr-ft²-°F
@Temperature 68.0 - 1110 °F
Maximum Service Temperature, Air 1800 °C3270 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.70 - 0.800.70 - 0.80

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TIMET TIMETAL® 679 (Ti-11Sn-5Zr-2.25Al-1Mo-0.2Si) Titanium Alloy; Air Cooled & Aged
Molybdenum Disilicide, MoSi2
Overview of materials for Stainless Steel
Vitreous Carbon (Glassy Carbon)
Overview of materials for T 300 Series Stainless Steel

NSANDV5032 / 199596

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.