MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Surlyn® 9945 Thermoplastic Ionomer Resin
Categories: Polymer; Thermoplastic; Ionomer; Ionomer, Molded

Material Notes: Surlyn® 9945 provides high flow properties and consistent, easy processing behavior in molded and extruded applications. It is positioned in the medium/high acid, high neutralization area of the ionomer spectrum.

Surlyn® 9945 is ideal for applications where fast molding cycles at reduced molding temperatures are desired. The high flow characteristics also facilitate molding in thin sections. Surlyn® 9945 is used primarily in blends with other ionomers, such as Surlyn®8945, to provide improved cut resistance and impact durability, as well as increased resiliency and coefficient of restitution.

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/ccASTM D792
Melt Index of Compound 4.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ASTM D2240
Tensile Strength at Break 19.3 MPaASTM D638
Tensile Strength, Yield 13.8 MPaASTM D638
Elongation at Break 300 %ASTM D638
Flexural Modulus 0.338 GPaASTM D790(B)
 
Thermal PropertiesOriginal ValueComments
Melting Point 51.0 - 89.0 °CASTM D3418(DSC)
Vicat Softening Point 71.0 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Surlyn® 8945 Thermoplastic Ionomer Resin
Dow Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film
Dow Surlyn® 1650SB
Dow Surlyn® SG201U NC010 Supergloss Molding Alloy
Dow Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating

PDUPM102 / 33769

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.