MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Karina 802-27/13-IS-RG Smoky Clear PVC Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Molded

Material Notes:

Information provided by Karina Indústria e Comércio de Plásticos Ltda.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 - 1.37 g/ccASTM D 792
ASTM Color -1.31 - 4.69Color A, ME 12
 3.54 - 9.54Color B, ME 12
 67.56 - 73.56Color L, ME 12
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78 - 82
@Time 15.0 sec
ASTM D 2240
Tensile Strength >= 550 kg(f)/cm²ASTM D 638
 
Descriptive Properties
ApplicationGeneral Purpose Injection Molded Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Sinvicomp DBS 5608 Polyvinyl Chloride, Rigid
Teknor Apex APEX® SRP 2700A Polyvinyl Chloride, Rigid
Teknor Apex APEX® SIC 3705 Rigid Polyvinyl Chloride
Teknor Apex APEX® RE 8114 UV Polyvinyl Chloride, Rigid
Karina E 830-10/150-Y-ERYB-LMP White PVC Compound

PKARIN9210 / 170866

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.