MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Thermal Ceramics Superwool 607 Flex-Wrap Paper
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Superwool Papers are uniquely designed from Superwool bulk and organic binders in a unique paper making process. Superwool Papers are specially processed to offer excellent performance in high-temperature applications. Superwool Papers offers an alternative to traditional solutions due to its unique properties of high refractoriness and excellent nonwetting characteristics to applications requiring direct contact with molten aluminum.

Superwool provides stability and resistance to chemical attack. Exceptions include hydrofluoric acid, phosphoric acid and strong alkalis (i.e. NaOH, KOH). Superwool is unaffected by incidental spills of oil or water. Thermal and physical properties are restored after drying.

Superwool Papers has excellent tensile strengths, high insulating values at high temperatures, and outstanding handling characteristics. It conforms easily to complex shapes and can be die-cut.

Features:

  • Low biopersistence
  • Thin, flexible high temperature insulation
  • Thermal stability
  • Conforms easily to complex shapes
  • Low heat storage
  • Easily die-cut to form complex shapes for high temperature gasketing
  • Flexible and resilient
  • Immune to thermal shock
  • Excellent thermal insulating performance
  • Based on patented technology
  • Low thermal conductivity and heat storage
  • Non-wetting to molten aluminum
  • Applications:

  • Gasketing between aluminum and zinc trough sections
  • Aluminum furnace tap-out plug cover and parting agent
  • Aluminum distributor pan linings
  • Gaskets for any high temperature application
  • Back up lining for metal troughs
  • Refractory back up for aluminum melting and holding furnaces
  • Aluminum casting and fabrication
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.160 - 0.208 g/cc0.00578 - 0.00751 lb/in³
    Loss On Ignition 2.0 - 5.0 %2.0 - 5.0 %
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Ultimate 0.0345 - 0.0689 MPa5.00 - 10.0 psiFired
     0.207 - 0.345 MPa30.0 - 50.0 psi
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0562 W/m-K
    @Temperature 260 °C
    0.390 BTU-in/hr-ft²-°F
    @Temperature 500 °F
    ASTM C201
     0.0937 W/m-K
    @Temperature 538 °C
    0.650 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
    ASTM C201
     0.150 W/m-K
    @Temperature 816 °C
    1.04 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
    ASTM C201
     0.195 W/m-K
    @Temperature 982 °C
    1.35 BTU-in/hr-ft²-°F
    @Temperature 1800 °F
    ASTM C201
    Melting Point 1275 °C2327 °F
    Maximum Service Temperature, Air 1000 °C1832 °F
     
    Component Elements PropertiesMetricEnglishComments
    CaO 25 - 35 %25 - 35 %
    MgO 4.0 - 7.0 %4.0 - 7.0 %
    Other 1.0 %1.0 %
    SiO2 60 - 70 %60 - 70 %
     
    Descriptive Properties
    Alumina Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    CTHERM293 / 2613

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.