MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Multibase Multi-Flex® TPE A 7521 BLK
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Ash is 36%. Multi-Flex TPE contains Kraton™ G.

Data provided by Multibase.

Key Words: Thermoplastic Elastomer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ASTM D792
Melt Flow 10 g/10 min10 g/10 min(Condition L) ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 797910 sec; ASTM D-2240
Tensile Strength, Ultimate 6.20 MPa899 psiASTM D412
Elongation at Break 850 %850 %ASTM D412
Flexural Modulus 0.0560 GPa8.12 ksimethod 1, Proc.B; ASTM D-790
Tear Strength 35.0 kN/m200 pliASTM D624

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Reade Advanced Materials Indium-Tin Oxide (ITO) Powder (In2O3:SnO2)
Phillips 66 FC Fluid-D ISO Grade 46
OMG Americas GlidCop® AL-60 Dispersion Strengthened Copper
Multibase Multi-Flex® TPE A 6006 BLK
Multibase Multi-Flex® TPE A 6001 BLK

PLA055 / 49516

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.