MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay Chemicals 33% - Technical Grade Hydrochloric acid
Categories: Fluid

Material Notes: Supplied with HCl content of 33% to 36% by weight; property data specifically for HCl aqueous solution of 33%. Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regenerating, pickling or cleaning agent.

EINECS: 231-595-7/CAS: 7647-01-0/UN: 1789

Information provided by Solvay

Key Words: Muriatic Acid
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity  1.1 cP
@Temperature 60.0 °C
1.1 cP
@Temperature 140 °F
Dynamic Viscosity
 1.39 cP
@Temperature 40.0 °C
1.39 cP
@Temperature 104 °F
Dynamic Viscosity
 1.87 cP
@Temperature 20.0 °C
1.87 cP
@Temperature 68.0 °F
Dynamic Viscosity
 2.23 cP
@Temperature 10.0 °C
2.23 cP
@Temperature 50.0 °F
Dynamic Viscosity
 2.72 cP
@Temperature 0.000 °C
2.72 cP
@Temperature 32.0 °F
Dynamic Viscosity
 3.42 cP
@Temperature -10.0 °C
3.42 cP
@Temperature 14.0 °F
Dynamic Viscosity
Molecular Weight 36.47 g/mol36.47 g/molHCl
Vapor Pressure  0.00600 bar
@Temperature -10.0 °C
4.50 torr
@Temperature 14.0 °F
 0.0140 bar
@Temperature 0.000 °C
10.5 torr
@Temperature 32.0 °F
 0.0270 bar
@Temperature 10.0 °C
20.3 torr
@Temperature 50.0 °F
 0.0510 bar
@Temperature 20.0 °C
38.3 torr
@Temperature 68.0 °F
 0.160 bar
@Temperature 40.0 °C
120 torr
@Temperature 104 °F
 0.460 bar
@Temperature 60.0 °C
345 torr
@Temperature 140 °F
Surface Tension  0.067 dynes/cm
@Temperature 60.0 °C
0.067 dynes/cm
@Temperature 140 °F
 0.068 dynes/cm
@Temperature 40.0 °C
0.068 dynes/cm
@Temperature 104 °F
 0.070 dynes/cm
@Temperature 10.0 °C
0.070 dynes/cm
@Temperature 50.0 °F
 0.070 dynes/cm
@Temperature 20.0 °C
0.070 dynes/cm
@Temperature 68.0 °F
 0.071 dynes/cm
@Temperature 0.000 °C
0.071 dynes/cm
@Temperature 32.0 °F
 0.072 dynes/cm
@Temperature -10.0 °C
0.072 dynes/cm
@Temperature 14.0 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  2.30 J/g-°C
@Temperature -10.0 °C
0.550 BTU/lb-°F
@Temperature 14.0 °F
 2.40 J/g-°C
@Temperature 0.000 °C
0.574 BTU/lb-°F
@Temperature 32.0 °F
 2.40 J/g-°C
@Temperature 10.0 °C
0.574 BTU/lb-°F
@Temperature 50.0 °F
 2.50 J/g-°C
@Temperature 20.0 °C
0.598 BTU/lb-°F
@Temperature 68.0 °F
 2.60 J/g-°C
@Temperature 40.0 °C
0.621 BTU/lb-°F
@Temperature 104 °F
 2.70 J/g-°C
@Temperature 60.0 °C
0.645 BTU/lb-°F
@Temperature 140 °F
Thermal Conductivity  0.410 W/m-K
@Temperature -10.0 °C
2.85 BTU-in/hr-ft²-°F
@Temperature 14.0 °F
 0.430 W/m-K
@Temperature 0.000 °C
2.98 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
 0.440 W/m-K
@Temperature 10.0 °C
3.05 BTU-in/hr-ft²-°F
@Temperature 50.0 °F
 0.450 W/m-K
@Temperature 20.0 °C
3.12 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 0.470 W/m-K
@Temperature 40.0 °C
3.26 BTU-in/hr-ft²-°F
@Temperature 104 °F
 0.490 W/m-K
@Temperature 60.0 °C
3.40 BTU-in/hr-ft²-°F
@Temperature 140 °F
Melting Point -40.0 °C-40.0 °F
Boiling Point 76.0 °C
@Pressure 0.101 MPa
169 °F
@Pressure 14.6 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WSOLV138b / 234781

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.