MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Orgalloy® LT 5050 T6L NAT PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Property data for dry samples, unless noted.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
 1.04 g/ccCond.; ISO 1183
Melt Flow 2.5 g/10 min
@Load 5.00 kg,
Temperature 235 °C
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55
@Time 15.0 sec
Dry; ISO 7619-1
Elongation at Break >= 50 %Cond.; ISO 527-1/-2
Tensile Modulus 500 MPaCond.; ISO 527-1/-2
50% Modulus 23.0 MPa
@Strain 50 %
Cond.; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Dry; ISO 179/1eU
 NB
@Temperature 23.0 °C
Cond.; ISO 179/1eU
Charpy Impact, Notched 75.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 80.0 kJ/m²
@Temperature 23.0 °C
Cond.; ISO 179/1eA
Tensile Creep Modulus, 1 hour 420 MPaCond.; ISO 899-1
Tensile Creep Modulus, 1000 hours 270 MPaCond.; ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.50e+13 ohm-cmCond.; IEC 60093
Surface Resistance >= 1.00e+15 ohmCond.; IEC 60093
Dielectric Constant 4.0
@Frequency 1e+6 Hz
Cond; IEC 60250
 4.0
@Frequency 100 Hz
Cond.; IEC 60250
Dielectric Strength 36.0 kV/mmDry; IEC 60243-1
 36.0 kV/mmCond.; IEC 60243-1
Dissipation Factor 0.050
@Frequency 1e+6 Hz
Cond.; 0
 0.11
@Frequency 100 Hz
Cond.; IEC 60250
Comparative Tracking Index 600 VCond.; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 170 µm/m-°CDry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 180 µm/m-°CDry; ISO 11359-1/-2
Melting Point 220 °C10°C/min; Dry; ISO 11357-1/-3
Vicat Softening Point 75.0 °C50°C/h 50N; Dry; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection Molding; ISO 294
Mold Temperature 60.0 °CInjection Molding; ISO 10724
 
Descriptive Properties
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
Moisture SensitiveYes
Processing MethodsCalandering
 Film Extrusion
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
 Thermoforming
 Transfer Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Orgalloy® LT 5050 ES BLACK Polyamide Alloy
Samyang Triel® 5652EM Thermoplastics Polyetherester Elastomer, Extrusion
Arkema Orgalloy® LE 60 THM NAT Polyamide Alloy
Arkema Orgalloy® LE 6000 ST NAT PA6
BASF Ultramid® B3K PA6 (Conditioned)

PARKF764 / 193550

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.