MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Lucas-Milhaupt Silvabrite® Lead-Free Solder
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy; Tin Alloy

Material Notes: Silvabrite silver/tin soldering alloys have been engineered specifically for field repair. These silver/tin solders have been specifically formulated to make difficult repairs swiftly and confidently. Use Silvabrite for fast melting, free flowing jobs. Silvabrite is an approved and widely used alloy for the plumbing and building industries

Applications:

Silver/tin solders are low temperature, lead-free solders that can be used on most ferrous and non-ferrous metals, including stainless steel, bronze, brass and, to a very limited extent, aluminum.

Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.374 g/cc7.374 g/cc
Density 7.39 g/cc0.267 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point 221 - 225 °C430 - 437 °F
Solidus 221 °C430 °F
Liquidus 225 °C437 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 221 - 232 °C430 - 450 °FSoldering Range
 
Component Elements PropertiesMetricEnglishComments
Other, total <= 0.15 %<= 0.15 %
Silver, Ag 4.0 %4.0 %
Tin, Sn 96 %96 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nihon Superior SN100C Lead-Free Solder Alloy
AIM SAC305 Lead-Free Solder for Photonic Packaging
Indium Corp. Indalloy® 254 86.9Sn/10.0In/3.1Ag Lead-Free Solder Alloy
Indium Corp. Indalloy® 256 96.5Sn/3.0Ag/0.5Cu Lead-Free Solder Alloy
Lucas-Milhaupt Silvabrite® 100® Lead-Free Solder

NBRW006 / 79782

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.