MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ConocoPhillips Hydroclear® 320 Multipurpose R&O Oil, AGMA Lubricant No. 6
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear Multipurpose R&O Oil is specially formulated with proprietary additive chemistry and is recommended for use in a variety of systems which require rust- and oxidation-inhibited oils. The added benefit of mild antiwear protection can significantly increase equipment life, particularly in these hardworking times. These applications include general oiling, air compressors, steam turbines, hydraulic systems, circulating oil systems, oil-filled couplings, centrifugal pumps and lightly loaded gearboxes. Hydroclear Multipurpose R&O Oil has been tested and formally approved by Cincinnati Milacron under specifications P-38 (ISO 32), P-55 (46) and P-54 (68). Hydroclear Multipurpose R&O Oil exceeds Vickers I-286-S requirements. Hydroclear Multipurpose R&O Oil 460 meets the requirements of the Morgoil Lubricant Specification for use in roll-neck bearings. Proven performance in turbines which require antiwear, such as ABB and Alstom (some). Excellent for mist lubrication systems.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.888 g/cc0.0321 lb/in³
Viscosity Measurement 9595Viscosity Index
Saybolt Viscosity at 100°F 1694 SUS1694 SUS
Saybolt Viscosity at 210°F 119 SUS119 SUS
Kinematic Viscosity at 40°C (104°F) 318 cSt318 cSt
Kinematic Viscosity at 100°C (212°F) 23.9 cSt23.9 cSt
Oxidative Stability 3000 hour3000 hour
ASTM Color 5.05.0
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.400 mm0.0157 in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 30.0 kV/mm762 kV/inNo thickness given
 
Thermal PropertiesMetricEnglishComments
Pour Point -15.0 °C5.00 °F
Rotating Bomb Oxidation Test (RBOT) 600 min600 minASTM D 2272
Flash Point 277 °C530 °F
 
Descriptive Properties
ASTM Rust A&BPass
Copper Corrosion1A
Emulsion Characteristics (40-40-0)25 minutes
FZGPass 9 Load StagesASTM D5182

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 Refrigerant Compressor Oil ISO Grade 100
ConocoPhillips Conoco® El Mar® Geo Low Ash Oil, SAE Viscosity Grade 15W-40
ConocoPhillips Conoco® El Mar® Ashless Supreme Oil, SAE Viscosity Grade 15W-40
ChevronTexaco ISO 680 Ultra Gear Lubricant
ChevronTexaco ISO 680 AIO

WCON105 / 75142

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.