MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Fainplast Compounds Propylplus HPB 011/5 Cable Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Specially designed for the production of cables that require high stability to heat degradation and superior electro-mechanic properties at high temperatures.

Information provided by Fainplast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 54
@Time 15.0 sec
54
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 15.0 MPa2180 psi50 mm/min; ISO 527
Elongation at Break 400 %400 %50mm/min; ISO 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 5.00e+15 ohm-cm
@Temperature 20.0 °C
>= 5.00e+15 ohm-cm
@Temperature 68.0 °F
Alternating Polarity Method; ASTM D257
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 24 %24 %IEC 4589
 
Descriptive Properties
Emission of Halogenidric Acids (%)< 22IEC 60754-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFAIN9872 / 282371

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.