MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman Llumar DL30GN SR PS (Green) Window Film
Categories: Polymer; Film

Material Notes: Deluxe films are specified for commercial buildings where high levels of heat rejection and glare reduction are needed. Deluxe films are ideal for privacy applications and exterior aesthetics. They are scratch-resistant, reduce 99% of ultraviolet rays, and come in gray and bronze.

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 33 %
UV Transmittance 32 %Solar
Reflection Coefficient, Visible (0-1) 0.14Visible Reflectance (exterior)
 0.14Visible Reflectance (interior)
 0.18Total Solar Reflectance
 
Descriptive Properties
% Glare Reduction63
% Summer Solar Heat Gain Reduction44
% Total Solar Energy Rejected52
% Ultraviolet Ray Protection (wavelengths 300-380nm)>99
% Winter Heat Loss Reduction5
Emissivity0.75
Light to solar gain (LSG)0.69
Shading coefficient0.53
Solar absorption50
Solar Heat Gain Coefficient0.48
U-value0.99Winter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5424 / 222618

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.