MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller Körapop 954 Marine Adhesive and sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Körapop 954 Marine is a one-component, elastic, solvent free adhesive and sealant specifically designed for exterior application in the marine and boat industry
  • Good adhesion to glass, many kinds of metal (zinc, aluminum, steel) varnished and primed surfaces. Bonds well to wooden materials, duroplastics and thermoplastics (except PE, PP, PTFE) and mineral surfaces
  • Usable for bonding of mineral glass in the ship and boat building industry
  • Good resistance to humidity, weathering and to temperatures from -40°C to +90°C (for short intervals up to +120°C)
  • Overpaintable in the wet-on-wet process

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 58after 4 weeks; DIN 53 505
Tensile Strength 3.20 MPa
@Thickness 2.00 mm
DIN 53 504
Elongation at Break 380 %DIN 53 504
Tear Strength 22.0 kN/mDIN 53 515
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 minSkin formation time
 
Descriptive Properties
ColorWhite, black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL220 / 317011

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.