MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NOVA Chemicals P743C Expandable Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: A high strength regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.

Applications: Styrocell P743C is used mainly for producing contour moldings with wall thickness less than 10 mm.

This grade complies with major European and US food contact regulatory regimes, including: European Community Directive 90/128/ECC, including 92/39EEC and 95/EC, relating to plastics materials and articles, intended to come into contact with foodstuffs.

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.620 g/cc0.0224 lb/in³
Density >= 0.0170 g/cc>= 0.000614 lb/in³Minimum achievable; Single stage per-expansion in continuous expander at atmospheric pressure
 0.0170 - 0.0400 g/cc0.000614 - 0.00145 lb/in³Normal molded density assuming cost optimized selection of processing conditions.
Bead Size 0.400 - 0.700 mm0.0157 - 0.0276 in
 0.360 - 0.850 mm0.0142 - 0.0335 inCLAM 2115
 
Chemical PropertiesMetricEnglishComments
Styrene Content <= 0.10 %<= 0.10 %Residual Styrene Monomer Content per CLAM 3122
Blowing Agent Content >= 5.9 %>= 5.9 %CLAM 3135

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOVA342 / 55240

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.