VESTAKEEP® 5000 P is an unreinforced, high-viscosity polyether ether ketone powder. The semi-crystalline polymer features superior thermal and chemical resistance. VESTAKEEP® 5000 P is of low flammability. VESTAKEEP® 5000 P is supplied as powder in boxes with moisture-proof polyethylene liners. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C. Pigmentation may affect the values. Dry properties listed below Industrial Sector: Automotive and Mobility, Aircraft and Aerospace, Energy, Oil and Gas Processing: Injection molding, Press and sintering, Coating Delivery form: Powder Resistance to: Heat (thermal stability), Fire / burn Additives: Unfilled Applications: Electrical and Electronical Processing: Scatter coating Special Characteristics: High viscosity Chemical Resistance: General chemical resistanceInformation provided by Evonik. |