MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
CHT AS1740R RTV, silicone adhesive sealant
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Description: This is a non-corrosive, neutral cure, 1-part, RTV (Room Temperature Vulcanizing) silicone adhesive sealant. It is one in a range of Alkoxy cure products which are solvent free. It exhibits excellent primerless adhesion to many substrates and cures at room temperature when in contact with atmospheric moisture to form a tough rubber. This product will not corrode copper or its alloys and is suitable for use with electronic components.

Key Features

  • UL recognized in file No. E334038
  • Contains UV tracer for visual inspection
  • Self leveling, adhesive liquid
Application: Including but not limited to, protecting car engine number, fiber optic cables, sealing cable entry into distribution box

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccBS ISO 2781
Brookfield Viscosity 55000 - 70000 cPMixed
Storage Temperature <= 40.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 27ASTM D2240-95
Tensile Strength 363 psiISO 37
Elongation at Break 400 %ISO 37
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.25e+15 ohm-cmASTM D-257
Dielectric Constant 2.6ASTM D-150
Dielectric Strength 457 V/milASTM D-149
Dissipation Factor 0.0019ASTM D-150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 294 µm/m-°C
Thermal Conductivity 0.180 W/m-K
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -60.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 18.0 minTack Free Time / Skin Formation
 72.0 hour
@Temperature 23.0 °C
3mm Depth
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceViscous liquid
ColorTranslucent
Cure typeAlkoxy
RheologySelf Level
Self BondingYes
Volume Coefficient of Thermal Expansion883 ppm/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL027 / 314510

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.