MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ExxonMobil ENABLE™ EN 33900 Adhesive and Sealant Applications Resin  (discontinued **)
Categories: Polymer; Adhesive; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Enable EN 33900 is a high flow, 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ExxonMobil Method
Viscosity 8340 cP
@Temperature 190 °C
8340 cP
@Temperature 374 °F
ASTM D3236
Butyl Acrylate Content 32.5 %32.5 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 444415s; ASTM D2240
Tensile Strength at Break 0.965 MPa140 psiASTM D638
Elongation at Break 135 %135 %ASTM D638
Flexural Modulus, 1% Secant 5.38 MPa780 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 60.0 °C140 °FPeak Melting Temperature; ExxonMobil Method
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil ENABLE™ EN 33330 Adhesive Resin
ExxonMobil EN 33330 Ethylene n-Butyl Acrylate Copolymer Resin
Dow Elvaloy® 3427 AC Ethylene and 27% Butyl Acrylate Copolymer

PEXB169 / 37474

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.