MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® R550H NT453 Nylon 66, 50% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Vydyne R550H NT453 is a general purpose, 50% glass-filled, heat-stabilized PA66 based resin designed for injection molding applications. R550H NT453 offers standard flow with a natural surface finish and maintains the excellent resistance typical of PA66 in chemicals, machine and motor oils, solvents, and gasoline.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/ccDAM; ISO 1183
Water Absorption 0.50 %
@Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.2 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 180 MPa50% RH; ISO 527-2
 240 MPaDAM; ISO 527-2
Elongation at Break 2.5 %DAM; ISO 527-2
 3.5 %50% RH; ISO 527-2
Tensile Modulus 12600 MPa50% RH; ISO 527-2
 16800 MPaDAM; ISO 527-2
Flexural Strength 270 MPa50% RH; ISO 178
 350 MPaDAM; ISO 178
Flexural Modulus 11200 MPa50% RH; ISO 178
 16000 MPaDAM; ISO 178
Poissons Ratio 0.40ISO 527-2
Izod Impact, Notched (ISO) 16.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 17.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 18.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 21.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 91.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 95.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 95.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 110 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 14.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 21.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cm
@Thickness 1.00 mm
DAM; IEC 60093
Dielectric Strength 20.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
Arc Resistance 120 - 180 sec
@Thickness 3.00 mm
PLC 5; ASTM D 495
Comparative Tracking Index 400 - 599 V
@Thickness 3.00 mm
IEC 60112
Hot Wire Ignition, HWI 7.0 - 15 secPLC 4; UL 746
 7.0 - 15 secPLC 4; UL 746
 15 - 30 secPLC 3; UL 746
High Amp Arc Ignition, HAI >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/minPLC 1; UL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 12.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 260 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 255 °CUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical 140 °C
@Thickness 0.750 mm
UL 746
 140 °C
@Thickness 1.50 mm
UL 746
 140 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 130 °C
@Thickness 0.750 mm
UL 746
 130 °C
@Thickness 1.50 mm
UL 746
 130 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 140 °C
@Thickness 0.750 mm
UL 746
 140 °C
@Thickness 1.50 mm
UL 746
 140 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 HB
@Thickness 0.750 mm
 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
Flame Spread 0.000 mm/min
@Thickness 2.00 mm
ISO 3795
Glow Wire Ignition Temperature 700 °C
@Thickness 0.750 mm
IEC 60695-2-13
 700 °C
@Thickness 1.50 mm
IEC 60695-2-13
 750 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 675 °C
@Thickness 0.750 mm
IEC 60695-2-12
 675 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 310 °CInjection
Middle Barrel Temperature 280 - 310 °CInjection
Front Barrel Temperature 280 - 310 °CInjection
Nozzle Temperature 280 - 310 °CInjection
Melt Temperature 285 - 305 °CInjection
Mold Temperature 65.0 - 95.0 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 4.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
Agency RatingsASTM, D6779 PA012G50
 EC, 1935/2004
 EU, 10/2011
 EU, 2023/2006
 FDA, 21 CFR 177.1500
 SAE, J1639 PA1116
AppearanceNatural Color
FeaturesCreep Resistant
 Good Flow
 Good Mold Release
 Heat Stabilized
 High Rigidity
 High Strength
 Lubricated
 Thermal Stability
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
Overview of materials for Nylon 63, 35% Glass-Filled
Envalior Arnite® TV4 290 PBT-GF50
EMS-Grivory Grilon® BK-50 PA6-GB50
EMS-Grivory Grilamid® LKN-5H PA12-GB50

PASCE9842 / 220943

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.