System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Zhejiang Juner PA-A6-1 MF25%
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, 20% Mineral Filled
Material Notes:
Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical Appliance
Information provided by Zhejiang Juner New Materials Co, Ltd.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.38
g/cc
GB-1033
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
66.0
MPa
GB-1040
Elongation at Break
3.0 %
GB-1040
Flexural Strength
110.6
MPa
GB-9341
Flexural Modulus
5.82
GPa
GB-9341
Charpy Impact, Notched
0.550
J/cm²
GB-1043
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+15
ohm-cm
GB-1410
Comparative Tracking Index
550
V
GB4207
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
154
°C
GB-1634
Flammability, UL94
V-2
Processing Properties
Original Value
Comments
Processing Temperature
220
-
250
°C
Mold Temperature
60.0
-
90.0
°C
Drying Temperature
110
-
120
°C
@Time 14400 - 18000 sec
Injection Pressure
80.0
-
120
MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PJUNER13 / 48526
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.