MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

UNS C96400, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, and Sand.

Applications: Valves, pump bodies, flanges, elbows used for sea-water corrosion resistance.

Classified under: Copper-nickels

Typical data for sand-cast test bars. Alloy does not respond to heat treating

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 1401403000 kg
Tensile Strength, Ultimate 470 MPa68200 psi
Tensile Strength, Yield 255 MPa
@Strain 0.5 %
37000 psi
@Strain 0.5 %
Elongation at Break 28 %28 %in 50 mm
Modulus of Elasticity 145 GPa21000 ksi
Fatigue Strength 125 MPa
@# of Cycles 1.00e+8
18100 psi
@# of Cycles 1.00e+8
Reverse Bending
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Charpy Impact 106 J78.2 ft-lbV-notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00003448 ohm-cm
@Temperature 20.0 °C
0.00003448 ohm-cm
@Temperature 68.0 °F
as-cast tempers
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 - 300 °C
8.89 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.375 J/g-°C0.0896 BTU/lb-°F
Thermal Conductivity 29.0 W/m-K
@Temperature 20.0 °C
201 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1170 - 1240 °C2140 - 2260 °F
Solidus 1170 °C2140 °F
Liquidus 1240 °C2260 °F
Shrinkage 1.9 %1.9 %Patternmaker's Shrinkage
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Copper, Cu 65 - 69 %65 - 69 %
Iron, Fe 0.25 - 1.5 %0.25 - 1.5 %
Lead, Pb <= 0.030 %<= 0.030 %
Manganese, Mn <= 1.5 %<= 1.5 %
Nickel, Ni 28 - 32 %28 - 32 %
Niobium, Nb (Columbium, Cb) 0.50 - 1.5 %0.50 - 1.5 %
Silicon, Si <= 0.50 %<= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy
DIAB Divinycell® HCP 50 Polymer Foam
Nickel Aluminum Bronze, UNS C63200
Special Metals INCONEL® Alloy 625
Special Metals MONEL® Alloy 400

MC96400b1 / 11971

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.