MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SABIC LNP™ THERMOCOMP™ Compound MF006SXP Polypropylene, Unspecified (PP, Unspecified) (Americas)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: LNP THERMOCOMP MF006SXP compound is based on Polypropylene (PP) resin containing 30% glass fiber. Added features of this grade include: Heat Stabilized.

Features: High Stiffness,Heat Stabilized,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ASTM D792
 1.13 g/cc0.0408 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %23°C/50% RH/24 hrs; ASTM D570
 0.0300 %0.0300 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/in24hrs; ASTM D955
 0.0050 cm/cm0.0050 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0096 cm/cm0.0096 in/in24hrs; ISO 294
 0.010 cm/cm0.010 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 88.0 MPa12800 psiASTM D638
 91.0 MPa13200 psiISO 527
Elongation at Break 3.0 %3.0 %ASTM D638
 3.2 %3.2 %ISO 527
Tensile Modulus 7.30 GPa1060 ksi50 mm/min; ASTM D638
 7.60 GPa1100 ksi1 mm/min; ISO 527
Flexural Strength 139 MPa20200 psiASTM D790
 159 MPa23100 psiISO 178
Flexural Modulus 6.20 GPa899 ksiASTM D790
 8.70 GPa1260 ksiISO 178
Izod Impact Notched 117 J86.3 ft-lbASTM D256
Izod Impact, Unnotched 7.04 J/cm13.2 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²5.23 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²21.4 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 3.00 J2.21 ft-lbpeak; ASTM D3763
Impact Test 2.00 J1.48 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 60 - 120 sec60 - 120 secASTM D495
Comparative Tracking Index >= 600 V>= 600 VUL 746A
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness >=1.00 mm
15 - 30 sec
@Thickness >=0.0394 in
UL 746A
 30 - 60 sec
@Thickness >=3.00 mm
30 - 60 sec
@Thickness >=0.118 in
UL 746A
High Amp Arc Ignition, HAI  15 - 30 arcs
@Thickness >=1.00 mm
15 - 30 arcs
@Thickness >=0.0394 in
UL 746A
 60 - 120 arcs
@Thickness >=1.50 mm
60 - 120 arcs
@Thickness >=0.0591 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min0.394 - 1.00 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  26.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
14.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 26.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
14.7 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  59.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 59.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
@Thickness 3.20 mm
320 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 152 °C306 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 150 °C
@Thickness 3.20 mm
302 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 65.0 °C149 °FUL 746B
UL RTI, Mechanical with Impact 65.0 °C149 °FUL 746B
UL RTI, Mechanical without Impact 65.0 °C149 °FUL 746B
Flammability, UL94 HB
@Thickness >=1.00 mm
HB
@Thickness >=0.0394 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 215 - 225 °C419 - 437 °F
Zone 3 240 - 250 °C464 - 482 °F
Melt Temperature 225 - 250 °C437 - 482 °FInjection Molding
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81720 / 289667

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.