MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow AFFINITY™ SE 1400 Polyolefin Plastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: AFFINITY® SE 1400 polyolefin plastomer is an ethylene octene resin that offers excellent performance for profile extrusion of thick tubes and good melt strength for low shear blow molding. It has exceptionally high clarity and toughness. AFFINITY SE 1400 polymer has excellent compatibility with other polyolefins, allowing efficient blending and coextrusion. AFFINITY PF 1140 polymer complies with FDA regulation 21 CFR 177.1520c3.1b, which allows for its use in direct food contact applications.

Data provided by Dow Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.895 g/cc
Melt Flow 1.6 g/10 min
@Load 2.16 kg
Melt flow ratio I10/I2 is 10.2.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 89
Tensile Strength, Ultimate 43.4 MPa
Tensile Strength, Yield 5.20 MPa
Elongation at Break 710 %
Modulus of Elasticity 0.172 GPaMolded Sample 2% Secant Modulus
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 80.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow AFFINITY™ EG 8150 Polyolefin Elastomer
Dow Engage® Polyolefin Elastomer
Dow AFFINITY™ SM 8400 Polyolefin Elastomer
Dow AFFINITY™ VP 8770 Polyolefin Plastomer
Dow AFFINITY™ EG 8100 Polyolefin Elastomer

PDW408 / 34477

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.