CHT SilSo Cool 21012 Silicone Elastomer
Categories:
Polymer
;
Thermoset
;
Silicone
Material Notes:
Description: This is a two-component, 100% silicone solids, thermally conductive elastomer designed for electronic potting and roller applications.
Key Features
Comparative Tracking Index (CTI) > 600 V (PLC 0)
Information provided by CHT Group
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
2.30
g/cc
0.0831
lb/in³
A
2.30
g/cc
0.0831
lb/in³
B
2.30
g/cc
0.0831
lb/in³
Cured Product
Brookfield Viscosity
1500
cP
1500
cP
A
1500
cP
1500
cP
B
1500
cP
1500
cP
Mixed
Mechanical Properties
Metric
English
Comments
Hardness, Shore OO
71
71
ASTM D2240-95
Tensile Strength
<=
2.00
MPa
<=
290
psi
ISO 37
Elongation at Break
10 %
10 %
ISO 37
Tear Strength
<=
2.00
kN/m
<=
11.4
pli
BS ISO 34-1
Processing Properties
Metric
English
Comments
Cure Time
10.0
min
@Temperature 100 °C
0.167
hour
@Temperature 212 °F
Pot Life
>=
1440
min
>=
1440
min
Descriptive Properties
Appearance
white
Color
white
A
white
B
white
Cured Product
Mix Ratio
1:1
By Weight
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PCHTSIL081 / 314564
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.