MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Cosmic Plastics FARBOSET® 9081 Epoxy Powder
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: Cosmic FARBOSET 9081 is a nonanhydride, epoxy powder coating designed for low temperature applications for heat sensitive electronic components.

Applications: This compound is designed ideally suited for film and ceramic capacitors which need to be processed in low temperatures. It can be applied using fluidized bed, wheel coaters, or electrostatic spray techniques.

Information provided by Cosmic Plastics Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.54 g/cc0.0556 lb/in³Molded
Water Absorption 0.130 %
@Time 86400 sec
0.130 %
@Time 24.0 hour
Particle Mesh Size <= 80.0 Mesh<= 80.0 Mesh1%
 325 Mesh325 Mesh27-33%
Storage Temperature 18.0 °C64.4 °F
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.0
@Frequency 1000 Hz
4.0
@Frequency 1000 Hz
ASTM 150
Dielectric Strength 35.4 kV/mm900 kV/inASTM 149
Dissipation Factor 0.00600
@Frequency 1000 Hz
0.00600
@Frequency 1000 Hz
ASTM 150
Dielectric Loss Index 0.0140
@Frequency 1000 Hz
0.0140
@Frequency 1000 Hz
ASTM 150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C27.8 µin/in-°F
Glass Transition Temp, Tg 110 °C230 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 150 °C
0.167 hour
@Temperature 302 °F
 20.0 min
@Temperature 160 °C
0.333 hour
@Temperature 320 °F
 60.0 min
@Temperature 110 °C
1.00 hour
@Temperature 230 °F
Gel Time 0.583 min
@Temperature 150 °C
0.583 min
@Temperature 302 °F
Hot Plate
Shelf Life  4.00 Month
@Temperature 21.0 °C
4.00 Month
@Temperature 69.8 °F
 12.0 Month
@Temperature 4.00 °C
12.0 Month
@Temperature 39.2 °F
 
Descriptive Properties
Edge Coverage30%ASTM D-2967
Plate Flow23 mm150°C (302°F) / 60° angle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOSM033d / 325082

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.