MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Akrochem PROAID® AC-740 Process Aids
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Proaid AC-740 is a mixture of dark aromatic hydrocarbon resins designed to act as a unique processing aid for homogenizing polymer blends. It is quickly absorbed by the polymer matrix by wetting out the surfaces which leads to fast incorporation of other compound ingredients. Proaid AC-740 is best added at the beginning of the mix cycle to achieve the optimum effects.

Applications: The dosage for Proaid AC-740 is 4 to 15 phr. Proaid AC-740 may be used:

  • Primary Function: To greatly improve homogeneity of polymer blends of different polarities or different viscosities.
  • To increase green tack of compounds by showing some synergism with tackifying resins.
  • For reduction of viscosity which assists down line processing, in particular milling and calendering.
  • Due to its dark color, AC-740 is not recommended for light colored compounds.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/cc
Ash <= 2.0 %<= 2.0 %
 
Thermal PropertiesMetricEnglishComments
Softening Point 95.0 - 110 °C203 - 230 °F
 
Descriptive Properties
Appearancedark brown pastilles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH358 / 315276

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.