MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Barlog Plastics KEBABLEND TC FE 190802 Thermally Conductive PPS
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler

Material Notes: KEBABLEND / TC FE 190802 PPS is a functionalized compound based on PPS, which is thermally conductive and electrically insulating.

Properties: dimensionally stable, electrically isolating, good chemical resistance, high continuous used temperature, High stiffness, hydrolysis stable, semi-crystalline, thermally conductive

Typical areas of application: Heat sink, Pumps and motors, Pump housing, Structural components, Connecting elements

Industries: Automotive, Household appliances, Industry, Mechanical Engineering, Furniture industry

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.84 g/cc0.0665 lb/in³ISO 1183-1
Linear Mold Shrinkage, Flow 0.00200 cm/cm0.00200 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.00650 cm/cm0.00650 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 115 MPa16700 psiISO 527-1
Elongation at Break 0.700 %0.700 %ISO 527-1
Modulus of Elasticity 18.5 GPa2680 ksiISO 527-1
Charpy Impact Unnotched 1.80 J/cm²8.57 ft-lb/in²ISO 179-1eU
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Strength 27.0 kV/mm686 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.00 W/m-K6.94 BTU-in/hr-ft²-°Fin plane; DIN EN 821
 1.10 W/m-K7.63 BTU-in/hr-ft²-°Fthrough plane; DIN EN 821
Melting Point 280 °C536 °FISO 11357-1/-3
Maximum Service Temperature, Air 200 °C392 °FContinuous; ISO 2578
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
IEC 60695-11-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 320 - 340 °C608 - 644 °F
Mold Temperature 140 - 180 °C284 - 356 °F
Drying Temperature 120 - 140 °C248 - 284 °F
Dry Time 4.00 - 8.00 hour4.00 - 8.00 hour
Moisture Content <= 0.0200 %<= 0.0200 %
Back Pressure <= 1.00 MPa<= 145 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBARLO466 / 326540

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.