MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Taiwan PU Corporation UR60 Polyester Urethane Rubber
Categories: Polymer; Thermoset; Polyurethane, TS; Rubber or Thermoset Elastomer (TSE)

Material Notes: UR60 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of conventional rubber manufacturing equipment and techniques to yield finished urethane parts.

Compounds of urethane rubber can be molded by compression, injection, and transfer molding procedures. Excellent mold definition is obtainable in press cures. The linear shrinkage of vulcanizates of UR varies somewhat with the type of loading, but, in general this value is approximately 1.5%, which is comparable to that of neoprene.

Excellent mold release is provided by lubricant of M-7 or silicone mold release lubricants, but indiscriminate use can cause poor flow and knitting problems.

Information provided by Taiwan PU Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/cc
Mooney Viscosity 35 - 65
@Temperature 100 °C
ML 1-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60
Tensile Strength at Break 3360 psi
Elongation at Break 640 %
300% Modulus 0.580 ksi
@Strain 300 %
Tear Strength 220 pliDie C
Compression Set 62 %
@Temperature 158 °C,
Time 79200 sec
 
Processing PropertiesOriginal ValueComments
Processing Temperature 305 - 340 °F
Cure Time 5.00 - 45.0 min
 
Descriptive Properties
ColorWhite to cream
Health HazardNone
OdorFaint, characteristic
Physical FormSolid
Storage StabilityExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epichlorohydrin Rubber (CO, ECO)
Overview of materials for Silicone Rubber
Propylene Oxide Rubber (GPO)
Taiwan PU Corporation UR50 Polyester Urethane Rubber
ATG s.r.l. EACM Ethylene-Acrylic Rubber

PTPU46 / 70902

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.