MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPV X9156B Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV X9165B is a high performance thermoplastic vulcanizate engineered for use in demanding building and construction applications. Sarlink TPV X9165B is a black, medium hardness; low density grade processing exceptional chemical resistance, compression set and low temperature performance. It can be easily processed by injection and 2k injection molding with typical applications including gaskets, seals, profiles, and tubing; complies with EN 681-2 for pipe seals.

Availability: Europe

Features: Fatigue Resistant; High Elasticity; Low Density; Low Specific Gravity; Medium Hardness; Medium Heat Resistance

Agency Ratings: EN 681-2-2000

Uses: Gaskets; Industrial Applications; Profiles; Rubber Replacement; Seals

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Multi Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.957 g/cc0.0346 lb/in³ISO 1183
Viscosity 280 cP
@Shear Rate 206 1/s,
Temperature 200 °C
280 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ISO 11443
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55
@Time 5.00 sec
55
@Time 0.00139 hour
ISO 868
 54.8
@Treatment Temp. 70.0 °C,
Time 605000 sec
54.8
@Treatment Temp. 158 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Tensile Strength at Break 4.50 MPa653 psiAcross Flow, Type 2; ISO 37
 4.94 MPa
@Treatment Temp. 70.0 °C,
Time 605000 sec
717 psi
@Treatment Temp. 158 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Elongation at Break 550 %550 %Across Flow, Type 2; ISO 37
 512 %
@Treatment Temp. 70.0 °C,
Time 605000 sec
512 %
@Treatment Temp. 158 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Compression Set  24 %
@Temperature 22.8 °C,
Time 259000 sec
24 %
@Temperature 73.0 °F,
Time 72.0 hour
ISO 815
 27 %
@Temperature 70.0 °C,
Time 79200 sec
27 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 35 %
@Temperature 100 °C,
Time 86400 sec
35 %
@Temperature 212 °F,
Time 24.0 hour
ISO 815
 46 %
@Temperature -10.0 °C,
Time 259000 sec
46 %
@Temperature 14.0 °F,
Time 72.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -58.9 °C<= -74.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 175 - 185 °C347 - 365 °F
Middle Barrel Temperature 180 - 205 °C356 - 401 °F
Front Barrel Temperature 195 - 210 °C383 - 410 °F
Nozzle Temperature 200 - 230 °C392 - 446 °F
Melt Temperature 200 - 230 °C392 - 446 °F
Mold Temperature 10.0 - 30.0 °C50.0 - 86.0 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hour
Back Pressure 0.500 - 1.00 MPa72.5 - 145 psi
Cushion 0.300 - 0.800 cm0.118 - 0.315 in
Screw Speed 100 - 200 rpm100 - 200 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1223 / 237714

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.