MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Dow Dow™ TCP-2495 NT HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Dow TCP-2495 NT HDPE is produced via UNIPOL™ Processing Technology. It is specifically designed for use in all duct and cable in conduit (CI) applications for both telecommunications and power cables. The natural resin combined with color concentrate can be readily processed by any current duct or conduit extrusion method in all sizes at commercial rates.
Industrial Standards Compliance: ASTM D 3350 – cell classification PE335440A

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: ASTM D 3350 PE335440A

Form: Pellets

Processing Method: Profile Extrusion

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.948 g/ccASTM D792
Environmental Stress Crack Resistance >= 3000 hourF0; ASTM D1693C
Melt Flow 0.21 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 21 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
PENT >= 10 hour
@Temperature 80.0 °C
ASTM F1473
Hardness, Shore D 68ASTM D2240
Tensile Strength at Break 5000 psiASTM D638
Tensile Strength, Yield 3300 psiASTM D638
Elongation at Break >= 1000 %ASTM D638
Flexural Modulus 125000 psiMethod I (3 point load); ASTM D790B
Izod Impact, Notched 2.00 ft-lb/inASTM D256A
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °F
Brittleness Temperature <= -139 °FASTM D746A
 
Processing PropertiesOriginal ValueComments
Melt Temperature 400 - 440 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF460 / 311153

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.