MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Petroquimica Triunfo Trithene® TU 8091 LDPE - Agricultural Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Trithene TU 8091 is a low-density polyethylene (LDPE) with high molecular weight, with excellent mechanical properties and good processability. These qualities ensure the production of very wide films with uniform thickness and excellent resistance to UV-radiation. The Trithene TU 8091 resin is stabilized with a synergistic combination of a hindered amine (HALS) with UV absorbers and antioxidants. The additive package warrants thermal and light stabilization for greenhouse mid-life films with very good resistance to the traditional soil disinfecting and crop protection chemicals normally applied in agriculture. This product complies with ASTM standard D1248-IA5.

Applications: Films for covering of greenhouses and both large and small tunnels. Films for applications that require high mechanical strength and high resistance to aging from solar radiation (UV radiation exposure).

Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.

Information provided by Dax Resinas

Petroquimica Triunfo has been acquired by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.922 - 0.924 g/ccASTM D1505
Thickness 50.0 microns
Melt Index of Compound 0.10 - 0.14 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 18.0 MPaASTM D638
Tensile Strength, Yield 11.0 MPaASTM D638
Film Elongation at Break, MD 595 %ASTM D882
Film Elongation at Break, TD 740 %ASTM D882
Elongation at Break 625 %ASTM D638
Secant Modulus, MD 0.0920 GPa5%; ASTM D882
Secant Modulus, TD 0.0910 GPa5%; ASTM D882
Coefficient of Friction, Dynamic 0.56ASTM D1894
Elmendorf Tear Strength, MD 8.80 g/micronASTM D1922
Elmendorf Tear Strength, TD 14.4 g/micronASTM D1922
Dart Drop Test 395 g(method A); ASTM D1709
Film Tensile Strength at Break, MD 20.0 MPaASTM D882
Film Tensile Strength at Break, TD 22.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 95.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 13 %ASTM D1003
Gloss 62 %@ 60° Gardner; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 195 °CMixture Zone
Feed Temperature 170 - 185 °C
Adapter Temperature 200 - 220 °C
Blow-up Ratio (BUR) 3.0Recommended

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 2024-T361
Aluminum 2024-O
Aluminum 201.0-T7, Sand Cast
Aluminum 1050A Composition Spec
Alclad Aluminum 2024-T861

PDAX093 / 29518

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.