Description: - Flexible, urethane-based magnetic absorber.
- Ideal for suppression in an enclosed cavity, signal isolation and surface current attenuation.
- Standard sheet size: 24” x 24” (30.48 cm x 30.48 cm); Custom sizes available upon request.
- Available with pressure sensitive adhesive(PSA).
- Can be water-jet or die cut for custom configurations.
- Halogen free, RoHS and REACH compliant.
Information provided by Hexcel Corporation. |