Description: This product is an industrial amine functionalized polydimethylsiloxane polymer. Key Features - Durable and abrasion resistant
- Easy spreading when cut in solvent
- Improved water repellency on surfaces
- Improved gloss
Key Applications- Automotive care
- Polishing applications
- Mold release
- Textiles
Application: ICM SF-721P is a 100% active aminofunctional polydimethylsiloxane. ICM SF-721P uses the polar nature of amino-functional silicones to deposit and adhere strongly to automobile finishes, chrome, aluminum surfaces, and textiles.Information provided by CHT Group |