MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Pyro-Putty™ 600 High Temperature Ceramic Adhesive/Paste, Alumina Filled  (discontinued **)
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and do not outgas after curing. They are also environmentally safe, non-flammable materials which contain no volatile organic compounds.

General Features: Ceramic Fiber-Reinforced
Bonding: Ceramic to Ceramic
Principal Use: Refractory Repair

Vendors: Aremco offers a range of adhesives formulated using a broad range of ceramics fillers and inorganic binders, and are ideal for bonding, potting and sealing ceramics, composites, graphite, refractory metals, quartz, and semiconductors. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.16 g/cc2.16 g/cc
Storage Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
 
Mechanical PropertiesMetricEnglishComments
Impact Test 11.3 J8.30 ft-lbTorque Strength; curing for 5 hrs at 200°F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  1e+05
@Temperature 538 °C
1e+05
@Temperature 1000 °F
 1.00e+9 ohm-cm
@Temperature 23.0 °C
1.00e+9 ohm-cm
@Temperature 73.4 °F
Dielectric Strength  3.15 kV/mm
@Temperature 538 °C
80.0 kV/in
@Temperature 1000 °F
 7.87 kV/mm
@Temperature 23.0 °C
200 kV/in
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 7.56 µm/m-°C
@Temperature 20.0 °C
4.20 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 1370 °C2500 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 300 - 420 min5.00 - 7.00 hour2-4 hrs Air Set; 3 hrs at 200°F
Shelf Life 6.00 Month6.00 Month

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Superwool® Inorganic Bonds and Shapes I-Superwool Plus Thermal Ceramic
Morgan Advanced Ceramics Superwool® Clad HT Thermal Ceramic
Morgan Advanced Ceramics High Strength Ceramic Fibre Boards SS 800 Ceramic Fibre Boards
Mid-Mountain Materials HYTEX® 2200 Ceramic Fiber Industrial Textile
Goodfellow Alumina Silicate SiO2 53/Al2O3 47

ZCAREM16 / 557

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.